A Fractographic Study of Fatigue Failures in Combat Aircraft Trailing Edge Flap Hinge Lug Bores in Both Test and Service Assets

Ben Main,Simon Barter, Ingrid Kongshavn, Ricardo Filipe do Rosario,Jason Rogers, Mirco Figliolino

Engineering Failure Analysis(2025)

引用 0|浏览1
关键词
Aerospace engineering,Aircraft,Aluminium alloys,Forging,Fractography,Fatigue,Fretting,Corrosion,Materials change