Microstructural Assessment of Molybdenum Disulfide Coatings Using Nanoindentation Hardness
ACS APPLIED MATERIALS & INTERFACES(2025)
关键词
MoS2,nanoindentation,density,hardness,crystallinity,friction,wear,PVD