Dissolution Behavior of Laves Phase and Its Interaction with Δ Phase in Superalloy 718 Fabricated by Wire Arc Additive Manufacturing
VACUUM(2025)
关键词
Superalloy,Isothermal heat treatments,Laves phase,Precipitation,Wire arc additive manufacturing