Oxygen-driven De-Alloying of Fe-14Cr-12Ni-10Mn-3Cu-2.5Al-1Nb Austenitic Steel at 500 °C in Static Pb-Bi Eutectic with Concentration of Dissolved Oxygen Alternating from ∼10-6 to 10-9 Mass% for 10000 H
CORROSION COMMUNICATIONS(2025)
Key words
Austenitic stainless steel,Corrosion,De-alloying,Liquid lead-bismuth eutectic,Oxidation