Microstructural Evolution and Nanoindentation Creep Behavior in a PdAgCuAuPtZn Multi-Principal Elements Alloy

JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T(2024)

Cited 0|Views1
Key words
Precious metals MPEA,Nanoindentation creep behavior,Discontinuous precipitation,Chemical short-range order,Spinodal decomposition