Enhancement of Catalytic Activity via Inevitable Reconstruction of the Ni-Mo Interface for Alkaline Hydrogen Oxidation.

Xiaoyun Song, Qimei Yang, Zebi Chen, Kaisheng Zou,Zhenyang Xie,Wei Ding,Zidong Wei

Small (Weinheim an der Bergstrasse, Germany)(2024)

引用 0|浏览10
暂无评分
摘要
The inevitable oxidation of nickel-metal-based catalysts exposed to the air will lead to instability and poor reproducibility of a catalytic interface, which is usually ignored and greatly hinders their application for the catalysis of alkaline hydrogen oxidation. The details on the formation of a world-class nickel-based HOR catalyst Ni3-MoOx/C-500 are reported via an interfacial reconstruction triggered by passive oxidation upon air exposure. Interfacial reconstruction, initiated with various Ni-Mo metal ratios and annealing temperature, can fine-tune the Ni-Mo interface with an increased work function and a reduced d-band center. The optimized Ni3-MoOx/C exhibits a record high mass activity of 102.8 mA mgNi -1, a top-level exchange current density of 76.5 µA cmNi -2, and exceptional resistance to CO poisoning at 1000 ppm CO for hours. The catalyzed alkaline exchange membrane fuel cell exhibits a maximum power output of 600 mW cm-2 and excellent stability, ranking it as one of the most active non-precious metals HOR catalysts to date.
更多
查看译文
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要