Predictive design of novel nickel-based superalloys beyond Haynes 282
Acta Materialia(2024)
摘要
Nickel-based superalloys are in great demand for harsh-service conditions involving high temperatures and oxidative environments. Haynes 282 stands out due to its excellent high-temperature properties and easy fabricability. However, the upper operation temperature of Haynes 282 is limited due to its relatively low liquidus temperature. Equipped with high-fidelity density-functional theory calculations and high-throughput experimentation methodology, we explored new compositional spaces that exhibit higher liquidus temperature and higher strength. While maintaining the manufacturability, the newly designed alloy shows improved strength and ductility at room temperature and better oxidation resistance up to 800°C. The new compositions showcase a minor change in the refractory and metalloid content can significantly impact the mechanical and oxidation performance of superalloys.
更多查看译文
关键词
Ni-based superalloys,DFT calculation,Mechanical properties,oxidation properties,Microstructure
AI 理解论文
溯源树
样例
![](https://originalfileserver.aminer.cn/sys/aminer/pubs/mrt_preview.jpeg)
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要