Mechanistic Crack Growth in Ni-Based Superalloy Single Crystal Gamma-Gamma Prime Microstructure: The Role of Stress, Temperature and Cubic SlipVasilis Karamitros, Thomas Bellamy, Duncan Maclaclan,Fionn P.E. Dunnecrossref(2024)引用 0|浏览1暂无评分AI 理解论文溯源树样例生成溯源树,研究论文发展脉络Chat Paper正在生成论文摘要