Microstructural Evolution and Creep Behavior of a Novel Ni-Fe-Based Superalloy Gh2070p for 700 °C Class A-Usc Steam Pipes
Journal of Alloys and Compounds(2024)
关键词
Ni-Fe-based superalloy,Creep,Microstructure,Deformation behavior