Nanoindentation Responses of Fe−Cr Alloys from Room Temperature to 600 °C
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING(2024)
Key words
High-temperature nanoindentation,Eurofer97,Ferritic-martensitic,Portevin-Le Chatelier effect,Dynamic strain aging