The effect of slag variability in the attempted manufacture of AYF (alite-ye'elimite-ferrite) cement clinker at both laboratory and pilot scale

CEMENT(2024)

Cited 0|Views5
No score
Abstract
The production of AYF (alite-ye'elimite-ferrite) clinker was tested at laboratory and semi-industrial scale using by-products from the metallurgical industry: AOD slag; ladle slag; and fayalitic slag. Alite could be produced with ye'elimite using fluorine originating from AOD (argon oxygen decarburisation) slag as a mineraliser. After a successful laboratory demonstration, the clinker production was scaled to a semi-industrial trial. It was discovered that the reason for the absence of alite formation in a semi-industrial demonstration was that the AOD slag from the specific batch did not perform the designed mineralisation effect for alite formation. This study demonstrates that alite-ye'elimite can be produced at 1260 °C at laboratory scale by using fluorine mineralisation originating from an industrial by-product – in this case, AOD slag. However, the utilisation of by-products for delicate reactions requires detailed determination of the properties of the slag, as the variability from the same source yields different clinker chemistries and mineral phases.
More
Translated text
Key words
Calcium sulphoaluminate cement,scale-up,clinkering,waste valorisation,alite,ye'elimite,AOD slag,mineralisation
AI Read Science
Must-Reading Tree
Example
Generate MRT to find the research sequence of this paper
Chat Paper
Summary is being generated by the instructions you defined