Reaction-induced nano-sized TiC in additive manufactured Ni-Co based superalloy
MATERIALS RESEARCH LETTERS(2024)
Abstract
Carbon nanofibers (CNFs) and graphene nanosheets (GNs) are introduced to obtain nano-sized TiC particles in a novel additive manufactured Ni-Co-based superalloy. The double strengthening effects of reaction-induced TiC and remaining CNFs/GNs are conceptualized in the present paper. The CNFs and GNs act as heterogeneous nucleation sites for the formation of uniformly distributed TiC nanoparticles, which inhibits the crack and homogenize the microstructure. Interestingly, the existence of remaining GNs/CNFs is revealed via 3D atom-by-atom tomographic reconstruction technology for the first time. This unique combination of nanoparticles and residual CNFs/GNs nanofillers has great potential to develop superalloys with excellent properties.
MoreTranslated text
Key words
Superalloy,graphene,carbon nanofiber,additive manufacture,composites
AI Read Science
Must-Reading Tree
Example
![](https://originalfileserver.aminer.cn/sys/aminer/pubs/mrt_preview.jpeg)
Generate MRT to find the research sequence of this paper
Chat Paper
Summary is being generated by the instructions you defined