Microstructure and properties of Co-Ni-Al-W /á superalloy fabricated via laser fusion of elemental powders
ADDITIVE MANUFACTURING(2023)
摘要
Ball-milled elemental Co, Ni, Al, and W powders were used to fabricate a Co-0.20Ni-0.11Al-0.08W (mole fraction) alloy via laser powder bed fusion (L-PBF). In the as-fused state, microstructural features present within the FCC-gamma Co-Ni-Al-W matrix - partially-melted W powders, W-deficient regions, and cracks - are investigated with respect to the laser scanning speed. Tungsten particles appear to block or deflect internal cracks, thus improving cracking resistance due to thermal cycling during laser fusion. However, W-deficient regions, which are also enriched with Ni and Al, can act as crack nucleation sites due to the brittleness of the 8-NiAl and eutectic microconstituents. A homogenous FCC-gamma Co-0.20Ni-0.11Al-0.08 W (mole fraction) solid solution is obtained after a solutionizing treatment at 1200 degrees C, as W-rich particles fully dissolve, and W-deficient regions homogenize, into the matrix. A gamma/gamma '-two-phase microstructure forms upon subsequent aging at 900 degrees C, whose creep resistance is measured at 850 degrees C: below 300 MPa, deformation is dominated by diffusional creep (consistent with a relatively fine grain size of 50-100 mu m) while above 300 MPa, it is controlled by dislocation creep. Using elemental powder blends is a viable method to create microstructurally-sound, creep-resistant Co-based gamma/gamma ' superalloys via L-PBF.
更多查看译文
关键词
Co -based superalloy,Selective laser melting,Microstructure,Crack,Creep
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要