Precise Design of TiO2@CoOx Heterostructure via Atomic Layer Deposition for Synergistic Sono-Chemodynamic Oncotherapy
ADVANCED SCIENCE(2024)
摘要
Sonodynamic therapy (SDT), a tumor treatment modality with high tissue penetration and low side effects, is able to selectively kill tumor cells by producing cytotoxic reactive oxygen species (ROS) with ultrasound-triggered sonosensitizers. N-type inorganic semiconductor TiO2 has low ROS quantum yields under ultrasound irradiation and inadequate anti-tumor activity. Herein, by using atomic layer deposition (ALD) to create a heterojunction between porous TiO2 and CoOx, the sonodynamic therapy efficiency of TiO2 can be improved. Compared to conventional techniques, the high controllability of ALD allows for the delicate loading of CoOx nanoparticles into TiO2 pores, resulting in the precise tuning of the interfaces and energy band structures and ultimately optimal SDT properties. In addition, CoOx exhibits a cascade of H2O2 -> O-2 ->O-2(-) in response to the tumor microenvironment, which not only mitigates hypoxia during the SDT process, but also contributes to the effect of chemodynamic therapy (CDT). Correspondingly, the synergistic CDT/SDT treatment is successful in inhibiting tumor growth. Thus, ALD provides new avenues for catalytic tumor therapy and other pharmaceutical applications.
更多查看译文
关键词
atomic layer deposition,carrier separation efficiency improvement,energy band structure adaptation,heterostructure,synergistic sono-chemodynamic oncotherapy
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要