Amorphous bismuth and GO co-doped WO3 electrochromic film with fast-switching time and long-term stability

DALTON TRANSACTIONS(2024)

Cited 0|Views5
No score
Abstract
The sol-gel process for fabricating electrochromic thin films is straightforward, offering advantages such as low cost and ease of compositional control. Herein we prepared GO-Bi-WO3 films with improved electrochromic performance using a simple sol-gel spin-coating method. The sample shows a fast-switching time (1.8 s for coloring and 1.8 s for bleaching), large optical modulation (85% at 630 nm), excellent stability (86.4% retention after 10 200 cycles), and high coloration efficiency (65.9 cm(2) C-1). This work indicates the electrochromic performance of WO3-based films can be enhanced by incorporating GO, which provides an effective strategy for the rapid, safe, and efficient fabrication of electrochromic thin films.
More
Translated text
AI Read Science
Must-Reading Tree
Example
Generate MRT to find the research sequence of this paper
Chat Paper
Summary is being generated by the instructions you defined