Surface Analysis Insight Note: Observations Relating to Photoemission Peak Shapes, Oxidation State, and Chemistry of Titanium Oxide Films

SURFACE AND INTERFACE ANALYSIS(2024)

Cited 1|Views12
Key words
component spectra,linear least squares,oxidation state,titania,XPS