In this work, β-Ga2O3 thin films were deposited by radio frequency (RF) magnetron sputtering technique. The effect of oxygen-argon flow ratio (OAFR) on the formation of Frenkel defect pairs was systematically analyzed. The Frenkel defect pairs would become abundant when the OAFR was 25:25 sccm, resulting in a severe damage in crystalline quality and an increase in the density of disorder. With the further increase of OAFR, Frenkel defect pairs would dramatically decrease or even vanish due to the significant reduction of oxygen vacancies (V0). Immediately after that, on the basis of avoiding the influence of Frenkel defect pairs inside the β-Ga2O3 films to the devices, the p-NiO/i-Ga2O3/n-GaN diode was fabricated from the as-prepared high-quality β-Ga2O3 film after post-deposition annealing as the electron-blocking layer. Subsequently, its electrical characteristics were investigated in detail which exhibited excellent rectification characteristics under all test temperatures. Correspondingly, the device achieved electroluminescence (EL) with a dominant sharp emission peak in the ultraviolet range (∼375 nm). In the end, the energy band diagram was used for in-depth analysis of the EL mechanism.
更多
查看译文
关键词
frenkel defect pairs,thin film,gan-based,light-emitting
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要