Stress corrosion cracking induced by the combination of external and internal hydrogen in Al-Zn-Mg-Cu alloy
SCRIPTA MATERIALIA(2024)
摘要
Stress corrosion cracking (SCC) behaviors induced by the combination of external and internal hydrogen (H) in an Al-Zn-Mg-Cu alloy were systematically investigated via in-situ 3D characterization techniques. SCC of the Al -Zn-Mg-Cu alloy could initiate and propagate in the potential crack region where the H concentration exceeded a critical value, in which the nanoscopic H-induced decohesion of eta-MgZn2 precipitates resulted in macroscopic cracking. External H that penetrated the alloy from the environment played a crucial role during the SCC of the Al-Zn-Mg-Cu alloy by generating gradient-distributed H-affected zones near the crack tips, which made Al alloys in water environment more sensitive to SCC. Additionally, the pre-existing internal H was driven toward the crack tips during plastic deformation. It was involved in the SCC and made contributions to both the cracks initiation and propagation.
更多查看译文
关键词
Stress corrosion cracking,Hydrogen embrittlement,Al -Zn -Mg -Cu alloy,X-ray tomography,External and internal hydrogen
AI 理解论文
溯源树
样例
![](https://originalfileserver.aminer.cn/sys/aminer/pubs/mrt_preview.jpeg)
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要