Novel Method for Image-Based Quantified in Situ Transmission Electron Microscope Nanoindentation with High Spatial and Temporal Resolutions
Micromachines(2023)
Key words
mechanical quantification,in situ TEM,nanoindentation,focused ion beam,MEMS chip