A Revisit to the Role of Mo in an MP35N Superalloy: an Experimental and Theoretical Study

JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY(2023)

Cited 9|Views2
Key words
Mo addition,Solid solution strengthening,Grain boundary softening,Local lattice distortion,First-principles simulations,Stacking fault energy,Deformation twin