Abstract
BaTiO nanoparticles were prepared by the hydrothermal method, and the effect of 1-(propyl-3-methoxysilyl)-3-methylimidazole chloride on the size of BaTiO particles was investigated. The obtained BaTiO was characterized by XRD, SEM, TEM, and Raman spectroscopy; and the dielectric properties of BaTiO ceramic sheets were tested. The results indicate that the spherical BaTiO-N prepared without an ionic liquid was in a tetragonal phase with an average particle size of 129 nm. When an ionic liquid was added, the size of the BaTiO-IL decreased and the degree of agglomeration increased. In addition, with increasing quantity of ionic liquid, the tetragonal-phase content of BaTiO-IL gradually decreased until complete transformation into cubic phase. The dielectric constant of the BaTiO-N ceramics was the highest, and the dielectric constant decreased with decreasing BaTiO particle size. Moreover, two types of BaTiO nanoparticles (bowl- and sea urchin-shaped) were prepared by changing the hydrothermal conditions and additives. The average particle size of the former was 92 nm, the tetragonal-phase content was 90%, and the dielectric constant was large; whereas the sea urchin-shaped BaTiO consisted of small particles in the cubic phase, and the dielectric constant was small.
More
Translated text
AI Read Science
Must-Reading Tree
Example
Generate MRT to find the research sequence of this paper
Chat Paper
Summary is being generated by the instructions you defined