Rapid Bonding of Ti3SiC2 and Ti3AlC2 by Pulsed Electrical Current Heating

Shen L [Shen Lu][ ], Xue JM [Xue Jianming][ ],Barsoum MW [Barsoum Michel W.][ ], Huang Q [Huang Qing][ ]

JOURNAL OF THE AMERICAN CERAMIC SOCIETY(2017)

Cited 0|Views0
No score
Abstract
Inspired by pressure resistance welding of metallic materials, herein we describe how two MAX phases—Ti3SiC2 and Ti3AlC2—were successfully joined by a rapid electric current heating method in a pulsed electric current sintering furnace. No welding agent was employed and the total processing time was less than 6 min. When the bulk temperature of the joint couple exceeded 1070°C, good joints, with shear strength above 50 MPa, were achieved in both homo- and heterojunction joints.