Experimental Research on Recovery of Fluorite from a Polymetallic Mine Tailing in Inner Mongolia

Di Wu, Hongling Wang,Qingbo Meng,Yude Gao, Xiaowen Yang, Xiaogang Zhang

Kuangchan zonghe liyong(2022)

Cited 0|Views0
No score
Abstract
Flotation tailings of a polymetallic mine in Inner Mongolia contain fluorite resources. Due to the influence of the tungsten-tin flotation reagent and the ore embedded characteristics in the early stage, the fluorite flotation concentrate grade is up to 92%, and the recovery is about 30%. The fluorite resources in the tailings were not effectively recovered. In this study, the beneficiation feed grade of fluorite was improved by waste disposal with pre-magnetic separation, and organic depressor HG-1 was used instead of acidified water glass. Under the condition of original ore CaF2 grade of 17.65%, the fluorite concentrate with CaF2 grade of 97.26% and recovery of 63.15% was obtained, which realized the comprehensive recovery of fluorite resources in tailings.
More
Translated text
Key words
tailings recovery,fluorite flotation,magnetic separation and waste disposal,depressor hg-1
AI Read Science
Must-Reading Tree
Example
Generate MRT to find the research sequence of this paper
Chat Paper
Summary is being generated by the instructions you defined