Structural and Functional Picosecond Laser Modification of the Nimonic 263 Superalloy in Different Environmental Conditions and Optimization of the Irradiation Process
MATERIALS(2023)
关键词
Nimonic 263,picosecond laser,surface modification,argon-rich atmosphere,nitrogen-rich atmosphere,Taguchi’s robust parameter design