Metal oxides are an important class of functional materials, and for many applications, ranging from solid oxide fuel/electrolysis cells, oxygen permeation membranes, and oxygen storage materials to gas sensors (semiconducting and electrolytic) and catalysts, the interaction between the surface and oxygen in the gas phase is central. Ubiquitous Si-impurities are known to impede this interaction, commonly attributed to the formation of glassy blocking layers on the surface. Here, the surface oxygen exchange coefficient (k ) is examined for Pr Ce O (PCO), a model mixed ionic electronic conductor, via electrical conductivity relaxation measurements, and the area-specific resistance (ASR) by electrochemical impedance spectroscopy. It is demonstrated that even low silica levels, introduced by infiltration, depress k by a factor 4000, while the ASR increases 40-fold and we attribute this to its acidity relative to that of PCO. The ability to fully regenerate the poisoned surface by the subsequent addition of basic Ca- or Li-species is further shown. This ability to not only recover Si-poisoned surfaces by tuning the relative surface acidity of an oxide surface, but subsequently outperform the pre-poisoned response, promises to extend the operating life of materials and devices for which the catalytic oxygen/solid interface reaction is central.
More
Translated text
Key words
Pr 0.1Ce 0.9O 2-δ,mixed ionic electronic conducting oxide,oxygen exchange kinetics,relative acidity,silica poisoning
AI Read Science
Must-Reading Tree
Example
Generate MRT to find the research sequence of this paper
Chat Paper
Summary is being generated by the instructions you defined