Neutron irradiation analysis, inductively coupled plasma mass spectrometry (ICPMS), and cathodoluminescence (CL) spectroscopy are used to investigate the influence of transmuted Ge incorporation on the luminescence properties of $\ensuremath{\beta}\text{\ensuremath{-}}{\mathrm{Ga}}_{2}{\mathrm{O}}_{3}$ single crystals. Calculations based on ${\mathrm{Ga}}_{2}{\mathrm{O}}_{3}$-neutron interaction reveal temporal variations of both Ge and Zn concentrations as a function of time during and after neutron irradiation. To produce a concentration of $5\ifmmode\times\else\texttimes\fi{}{10}^{18}\phantom{\rule{0.16em}{0ex}}\mathrm{Ge}\phantom{\rule{0.16em}{0ex}}\mathrm{donors}/\mathrm{c}{\mathrm{m}}^{3}$ from the neutron transmutation of Ga, the $\ensuremath{\beta}\text{\ensuremath{-}}{\mathrm{Ga}}_{2}{\mathrm{O}}_{3}$ crystal was irradiated for 27 h, which was accompanied by the incorporation of ${10}^{16}\phantom{\rule{0.16em}{0ex}}\mathrm{Zn}\phantom{\rule{0.16em}{0ex}}\mathrm{acceptors}/\mathrm{c}{\mathrm{m}}^{3}$. These calculated dopant concentrations are confirmed by ICPMS. The $\ensuremath{\beta}\text{\ensuremath{-}}{\mathrm{Ga}}_{2}{\mathrm{O}}_{3}$ crystals exhibit a UV band at 3.40 eV due to self-trapped holes (STHs) and two blue donor-acceptor pair (DAP) peaks at 3.14 eV (BL1) and 2.92 eV (BL2). In addition to the neutron-induced incorporation of substitutional Ge donors and Zn acceptors on Ga sites, Ga vacancies (${V}_{\mathrm{Ga}}$) were created by high-energy neutrons in the flux, which strongly enhanced the BL1 peak. The ${V}_{\mathrm{Ga}}$ acceptors compensate the neutron-induced Ge donors, making the ${\mathrm{Ga}}_{2}{\mathrm{O}}_{3}$ crystal highly resistive. Concurrent temperature-resolved CL measurements of the $\ensuremath{\beta}\text{\ensuremath{-}}{\mathrm{Ga}}_{2}{\mathrm{O}}_{3}$ before and after neutron irradiation reveal a twofold increase in both the STH and BL1 peaks. This result suggests that STHs are preferentially localized at an O site adjacent to ${V}_{\mathrm{Ga}}$, as theoretically predicted by Kananen et al. [Appl. Phys. Lett. 110, 202104 (2017).]. Analysis of the ${\mathrm{Ga}}_{2}{\mathrm{O}}_{3}$ CL temperature dependence reveals that the UV and BL1 bands after the neutron irradiation exhibit an equivalent activation energy of $100\ifmmode\pm\else\textpm\fi{}10\phantom{\rule{0.16em}{0ex}}\mathrm{meV}$ due to the presence of a neutron-induced defect that acts as an efficient competitive nonradiative recombination channel. The results also provide evidence that the BL1 and BL2 bands arise from different DAP pairs.
更多
查看译文
关键词
neutron transmutation,luminescence,defect-related
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要