Slow strain rates tests (SSRT) were conducted on hydrogen-containing specimens of PH13-8Mo maraging stainless steel. Hydrogen-assisted subcritical quasi-cleavage cracking was shown to take place during SSRT, thus accelerating material failure. Fractographic analysis showed that quasi-cleavage is composed of flat brittle areas and rougher areas. Using cross-sectional electron backscatter diffraction (EBSD) analysis of a secondary subcritically grown crack, we observed brittle cracks propagated across martensite blocks ahead the main crack tip. These cracks were stopped at high-angle boundaries. The crack direction was consistent with propagation along {100} type planes. High-resolution EBSD showed significant crystal lattice rotation, hence consequential plastic deformation, concentrated between the main crack tip and the cracks located ahead it. It is concluded that quasi-cleavage in the material investigated here consists of {100} cleavage cracks connected by ductile ridges. A discontinuous mechanism, involving re-initiation of new cleavage cracks ahead the main crack tip is suggested.
更多
查看译文
关键词
Hydrogen embrittlement,Fracture,Maraging steels,Electron backscattering diffraction (EBSD)
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要