Depth Profiling Via Nanoindentation for Characterisation of the Elastic Modulus and Hydraulic Properties of Thin Hydrogel Layers

JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS(2023)

Cited 2|Views12
Key words
Nanoindentation,Hydrogel thickness,Elastic modulus,Permeability