A Novel p-Type ZnCoxOy Thin Film Grown by Atomic Layer Deposition
NANOMATERIALS(2022)
摘要
Reported herein is the atomic layer deposition (ALD) of novel ternary ZnCoxOy films possessing p-type semiconducting behavior. The preparation comprises of optimized ZnO and Co3O4 deposition in sub-cycles using the commercially available precursors cyclopentadienylcobalt dicarbonyl (CpCo(CO)(2)), diethylzinc (DEZ) and ozone (O-3). A systematic exploration of the film's microstructure, crystallinity, optical properties and electrical properties was conducted and revealed an association with Zn/Co stoichiometry. The noteworthy results include the following: (1) by adjusting the sub-cycle of ZnO/ Co3O4 to 1/10, a spinel structured ZnCoxOy film was grown at 150 degrees C, with it exhibiting a smooth surface, good crystallinity and high purity; (2) the material transmittance and bandgap decreased as the Co element concentration increased; (3) the ZnCoxOy film is more stable than its p-type analog Co3O4 film; and (4) upon p-n diode fabrication, the ZnCoxOy film demonstrated good rectification behaviors as well as very low and stable reverse leakage in forward and reverse-biased voltages, respectively. Its application in thin film transistors and flexible or transparent semiconductor devices is highly suggested.
更多查看译文
关键词
atomic layer deposition (ALD), ZnCoxOy film, p-type metal oxides
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要