Tunable Solid Acid Catalyst Thin Films Prepared by Atomic Layer Deposition.
ACS applied materials & interfaces(2022)
摘要
Solid acid catalysts, including zeolites and amorphous silica-aluminas (ASAs), are industrially important materials widely used in the fuel and petrochemical industries. The versatility of zeolites is due to the Brønsted acidity of the bridging hydroxyl and shape selectivity that can be tailored during and after synthesis. This is in contrast to amorphous silica-alumina, where tailoring acidity is a major challenge as the Brønsted acid structure in ASA is still debated. In both cases, however, the pore size and acidity cannot be tuned independently, and this is particularly limiting in the application of biomass conversion, where zeolite pores are too small for the molecules of interest. Herein, we present a method using atomic layer deposition (ALD) to prepare thin films of solid acid materials where the ratio of Brønsted to Lewis acid sites can be tuned precisely. This capability, combined with the sub-nm pore size control afforded by ALD yields a powerful and flexible method for synthesizing solid acid catalysts inside virtually any mesoporous host. We demonstrate the utility of these materials in two acid-catalyzed reactions relevant to biomass conversion: (1) Meerwein-Ponndorf-Verley-Oppenauer (MPVO) reaction and dehydration of fructose and (2) cascade reaction of glucose to 5-hydroxymethylfurfural. Finally, we propose a plausible structure for the Brønsted acid sites in our materials based on infrared spectroscopy and solid-state nuclear magnetic resonance measurements and density functional theory calculations and argue that this same structure might apply to conventional ASAs as well.
更多查看译文
关键词
Brønsted acid,amorphous silica-alumina,atomic layer deposition,catalyst,density functional theory,in situ measurement
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要