Spherical nanoindentation stress–strain responses of SIMP steel to synergistic effects of irradiation by H and He ions
Nuclear Science and Techniques(2022)
摘要
A novel Fe-10Cr ferritic/martensitic steel called SIMP was chosen to investigate synergistic effects of H and He on the mechanical properties of structural materials for innovative nuclear energy systems. Sequential and separate irradiation experiments on SIMP steel specimens at room temperature using H and He ions with various energy levels were conducted to produce an ion deposition plateau at 300–650 nm. The indentation stress–strain responses were examined using spherical nanoindentation tests after the irradiation experiments. It was found that the sequential irradiation by He and H produced a higher indentation yield stress than separate irradiation, indicating that the hardening was enhanced by the synergy of the H and He irradiation. The micro-mechanism responsible for enhancing the hardening of the SIMP steel through the H and He synergy was investigated using Doppler broadening spectroscopy detection and transmission electron spectroscopy observations.
更多查看译文
关键词
H/He irradiation,Spherical nanoindentation,Bubbles,Dislocation loops
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要