Mechanism of improved intermediate temperature plasticity of nickel-base single crystal superalloy with hot isostatic pressing
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T(2021)
关键词
Single crystal superalloy, Hot isostatic pressing, Plasticity, Microporosity, Mechanical properties