Herein, two new cobalt and manganese-based polymers named as catena-Poly[[diaquabis(4-nitrobenzoato-kappa O-1)cobalt(II)]mu-pyrazine-kappa N-2:N'] ( COPNO2 ) and catena-Poly[[diaquabis(4-nitrobenzoato-KO1)mangane se(II)]-mu-pyrazine -kappa N-2:N'] (MNPNO2) were synthesized. The crystal structure of COPNO2 and MNPNO2 was determined and explored by X-rays diffraction method. O-H center dot center dot center dot O, C-H center dot center dot center dot pi, , N-O center dot center dot center dot pi, and pi center dot center dot center dot pi stacking interactions were the key aspects of the crystal packing of COPNO2, whereas for MNPNO2, O-H center dot center dot center dot O, C-H center dot center dot center dot pi, , and pi center dot center dot center dot pi stacking interactions were the key aspects of the crystal packing. The Hirshfeld surface (HS) studies were accomplished for further investigation of the intermolecular interactions. In addition to that, density functional theory (DFT) computations for COPNO2 and MNPNO2 had been carried out at MO6 functional, to obtain optimized geometries and double-check the experimental results. Moreover, DFT calculations at the MO6 level manifest excellent correlation with the experimental data, which validates the clarity of cobalt and manganese-based polymers. Frontier molecular orbital (FMO) findings were explored to describe nonlinear optical (NLO) properties. The energy gap of COPNO2 was 0.81 eV, while MNPNO2 was examined as 2.16 eV. The global reactivity parameters of COPNO2 and MNPNO2 were determined from the FMO energies. The global reactivity parameters showed that COPNO2 and MNPNO2 have the more donating ability. The NLO results of MNPNO2 (beta(rot) = 1259.17178a.u.) were observed better than COPNO2 (beta(rot) = 34,678.44833a.u.). We propose that this synergistic (experimental-computational) study of COPNO2 and MNPNO2 may deliver new ways for its exploitation as NLO material for hi-tech applications. (C) 2021 Published by Elsevier B.V.
MoreTranslated text
Key words
Coordination polymers, Spectroscopic studies, Synthesis, Crystal structure, Frontier molecular orbital, DFT
AI Read Science
Must-Reading Tree
Example
![](https://originalfileserver.aminer.cn/sys/aminer/pubs/mrt_preview.jpeg)
Generate MRT to find the research sequence of this paper
Chat Paper
Summary is being generated by the instructions you defined