Trace amount of ceria incorporation by atomic layer deposition in Co/CoOx-embedded N-doped carbon for efficient bifunctional oxygen electrocatalysis: Demonstration and quasioperando observations
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY(2021)
Abstract
As a promising class of alternatives to noble metal-based oxygen electrocatalysts, hybrids of metal/metal oxide (M/MO) and N-doped carbon have been widely explored. To address the often-insufficient catalytic activity of single M/MO-embedded N-C systems, researchers have introduced a second M/MO, usually via wet processes. In this work, we leverage the unique capability of atomic layer deposition (ALD) to enable the introduction of a trace amount of ceria throughout a Co/CoOx-embedded N-doped carbon nanostructure in a highly uniform and dispersed manner to maximize heterogeneous interfacial areas and thus catalytically active sites. An optimally prepared catalyst achieves an ORR onset potential of 0.95 V (0.1 M KOH) and an OER potential of 1.53 V at 10 mA cm(-2) (1 M KOH) and exhibits excellent cyclic durability. Quasi-operando observations reveal the multifaceted roles of the tiny amount of introduced ceria in facilitating electrocatalytic activity and enhancing durability. The ceria activates reactant adsorbates and transfers the activated intermediates to neighboring CoOx and electronically couples with Co and N species for enhanced catalytic activity. A high concentration of trivalent Ce state is readily and continuously restored during ORR/OER for an uninterrupted activation of reactants, also contributing to a highly stable reaction. (C) 2021 Hydrogen Energy Publications LLC. Published by Elsevier Ltd. All rights reserved.
MoreTranslated text
Key words
Atomic layer deposition,Bifunctional oxygen electrocatalysis,Quasi-operando XPS,Metal-organic framework,Ceria
AI Read Science
Must-Reading Tree
Example
Generate MRT to find the research sequence of this paper
Chat Paper
Summary is being generated by the instructions you defined