Determination of mechanical properties in multiphase bodies of extraterrestrial originis a fundamental task. In this work the hardness and Young’s modulus in the Seymchanpallasite were determined in kamacite α-Fe (Ni, Co), taenite γ-Fe (Ni, Co), plessite (α+γ),tetrataenite FeNi using nanoindentation technique. For the first time, the hardness andmodulus of elasticity of a two-phase nanostructure of cloudy zone FeNi+α-Fe(Ni,Co),formed as a result of very slow cooling (about 1 K/Myr), was determined.