Nanoindentation-induced deformation twinning in MAX phase Ti2AlN

Christophe Tromas, Salomé Parent, Wilgens Sylvain,Ludovic Thilly, Gilles Renou, Christopher Zehnder,Sebastian Schröders,Sandra Korte-Kerzel,Anne Joulain

Acta Materialia(2022)

引用 3|浏览18
暂无评分
摘要
Plastic deformation mechanisms have been investigated in the MAX phase Ti2AlN. Nanoindentation has been used to induce plastic deformation in a single grain, and a Transmission Electron Microscopy (TEM) lamella has been extracted in cross section through the indent by using Focused Ion Beam (FIB) technique. By combining TEM observations and automated crystal orientation mapping (ACOM), highly misoriented domains (HMD) have been revealed below a nanoindentation imprint. Thanks to a careful analysis of the relative crystal orientations between these HMD, {112¯2} and {112¯1} deformation twins have been identified for the first time in a MAX phase. Complex structures, involving secondary twinning or different {112¯2} twin variants have also been characterized.
更多
查看译文
关键词
MAX phase,Nanoindentation,Nanomechanical testing,Twinning
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要