Synthesis Of Homo- And Copolyesters Containing Divanillic Acid, 1,4-Cyclohexanedimethanol, And Alkanediols And Their Thermal And Mechanical Properties

POLYMER DEGRADATION AND STABILITY(2021)

引用 6|浏览1
暂无评分
摘要
Divanillic acid, the dimer of vanillic acid, has been widely used as an aromatic building block of bio-based polymers. In this study, a series of homo- and copolyesters composed of a methylated dialkoxydivanillic acid monomer with an alkoxy side-chain length of 1 or 4 carbon units, cyclohexanedimethanol, and an alkanediol with a chain length of 6, 8, or 12 carbon units was synthesized. The polyesters obtained exhibited high weight-average molecular weights in the range of 4.4 x 10(4) to 20 x 10(4) g/mol and degradation temperatures higher than 380 degrees C. Thermo-pressed films were prepared from all the polyesters. Their glass transition temperature and elongation-at-break values could be tuned from -1 to 120 degrees C and 3% to 1500%, respectively, by changing the lengths of the alkoxy side chain and the alkanediol as well as the composition of the copolyester. (C) 2021 Elsevier Ltd. All rights reserved.
更多
查看译文
关键词
Vanillin, Divanillic acid, Biphenyl, Side-chain length, Long-chain alkanediol, Bio-based polyester
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要