Low- and high-viscosity bulk-fill resin composites: a comparison of microhardness, microtensile bond strength, and fracture strength in restored molars.

Fabiana Mg França, Jonathan Gb Tenuti, Isabela P Broglio, Lara Ej Paiva,Roberta T Basting,Cecília P Turssi, Flávia Lb do Amaral,André F Reis,Waldemir F Vieira-Junior

Acta odontologica latinoamericana : AOL(2021)

引用 2|浏览5
暂无评分
摘要
The aim of this study was to compare low- and high-viscosity bulk-fill composites for Knoop microhardness (KHN), microtensile bond strength (MTBS) to dentin in occlusal cavities, and fracture strength (FS) in molars with mesialocclusal- distal restoration. Disk-shaped samples with different thicknesses (2 or 4 mm) of low-viscosity (SDR Flow, Dentsply) and high-viscosity bulk-fill composites (Filtek BulkFill, 3M ESPE; and Tetric-N Ceram Bulk Fill, Ivoclar Vivadent) were prepared for top and bottom KHN analysis (n=10). MTBS to dentin and fracture pattern was evaluated in human molars with occlusal cavities restored with (n=10): conventional nanocomposite (Z350XT, 3M ESPE), low-viscosity (Filtek Bulk-fill Flow, 3M ESPE) or high-viscosity bulk-fill composites (Filtek BulkFill). The FS and fracture pattern of human molar with mesial-occlusal-distal restorations submitted or not to thermomechanical cycling were investigated (n=10) using: intact tooth (control), and restoration based on conventional microhybrid composite (Z250, 3M ESPE), low-viscosity (SDR Flow) or high-viscosity bulk-fill composites (Filtek BulkFill). The data were submitted to split-plot ANOVA (KHN), one-way ANOVA (MTBS), two-way ANOVA (FS) followed by Tukey's test (α=0.05). For KHN, there was no significant difference for the resin composites between the top and bottom. For MTBS, no significant differences among the materials were detected; however, the low-viscosity composite presented lower frequency of adhesive failures. For FS, there was no significant difference between composites and intact tooth regardless of thermomechanical cycling. Low- and high-viscosity bulk-fill composites have comparable microhardness and microtensile bond strength when used in occlusal restorations. Likewise, the bulk-fill composites present similar fracture strength in molars with mesio-occlusal-distal restorations.
更多
查看译文
关键词
composite resins,dental restoration failure,hardness,viscosity
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要