Viscoplastic Constitutive Model of a Nickel-Based Superalloy under Multiaxial Loading Conditions

Journal of Iron and Steel Research International(2021)

引用 5|浏览1
关键词
Nickel-based alloy,Multiaxial loading,Viscoplastic constitutive model,Lemaitre damage model,Non-proportional hardening factor