Selected Spectroscopic Techniques for Surface Analysis of Dental Materials: A Narrative Review
MATERIALS(2021)
Abstract
The presented work focuses on the application of spectroscopic methods, such as Infrared Spectroscopy (IR), Fourier Transform Infrared Spectroscopy (FT-IR), Raman spectroscopy, Ultraviolet and Visible Spectroscopy (UV-Vis), X-ray spectroscopy, and Mass Spectrometry (MS), which are widely employed in the investigation of the surface properties of dental materials. Examples of the research of materials used as tooth fillings, surface preparation in dental prosthetics, cavity preparation methods and fractographic studies of dental implants are also presented. The cited studies show that the above techniques can be valuable tools as they are expanding the research capabilities of materials used in dentistry.
MoreTranslated text
Key words
dental materials,dental ceramics,spectroscopy,IR,FT-IR,Raman spectroscopy,UV-Vis,X-ray spectroscopy,XRF,XRD,MS
AI Read Science
Must-Reading Tree
Example
![](https://originalfileserver.aminer.cn/sys/aminer/pubs/mrt_preview.jpeg)
Generate MRT to find the research sequence of this paper
Chat Paper
Summary is being generated by the instructions you defined