采用无机盐溶胶-凝胶法制备了颗粒均匀的形态为针状的(Eu2+,Dy3+)SrAl2O4纳米粉体.通过TG-DTA分析和X射线衍射和扫描电镜分析方法,对样品进行了微观结构和表面形态的表征.研究了纳米(Eu2+,Dy3+)SrAl2O4粉体在不同烧结温度下固相反应过程和成相规律.实验结果表明,当样品的烧结温度为500 ℃时是单一的Sr(NO3)2晶相;750 ℃左右生成了Sr3Al2O6,并伴有少量SrAl2O4晶体;1 100 ℃是生成了结晶度良好的针状纳米(Eu2+,Dy3+)SrAl2O4粉体.通过计算,样品粉体晶粒平均为80~100 nm.该晶体粒度随烧结温度升高而逐渐变大.