Influence Of Shot Peening On Tensile Properties Of Dd6 Single Crystal Superalloy
Journal of Materials Engineering(2019)
摘要
The influence of cast steel shot-peening on the tensile properties of the second generation single crystal superalloy DD6 under 500, 600,650 degrees C was investigated by SEM, X-ray and TEM. The results show that the shot-peening has no influence on the tensile strength of DD6 alloy at 500, 600, 650 degrees C , and the yield strength is slightly increased, while the elongation and the shrinkage of cross section are remarkably decreased. The shot-peening DD6 alloy is ruptured after the flow stress rising to the highest point, and the cross section of fracture samples presents circle shape. The stress-strain curves of non-shot-peening DD6 alloy exhibit double stages feature, and the cross section of fracture samples presents ellipse shape.
更多查看译文
关键词
DD6, single crystal superalloy, shot-peening, tensile property, microstructure