固溶温度对Fe-24Al-Sn合金微观组织和力学性能的影响

Metallic Functional Materials(2017)

Cited 0|Views2
No score
Abstract
研究了不同固溶温度对Fe-24Al-Sn合金的微观组织和力学性能的影响.结果表明,与Fe-24Al合金相比,随着固溶温度从825℃增加到875℃,Fe-24Al-Sn合金的硬度逐渐从379HV增大到394HV,抗压强度逐渐从500 MPa降低到225 MPa,合金变脆.铸态合金的相结构为B2的FeAl相和Fe3Al相,还出现了Fe9Sn和Sn相.随着固溶温度的增加,合金中逐步发生B2→DO3 (Fe3 Al)的相变.