40Cr热轧棒线材的生产实践
Sichuan Metallurgy(2017)
Abstract
水钢采用100t转炉—LF炉精炼—150mm×150mm方坯连铸—高速线材轧制或棒材轧制的工艺流程生产出了φ10~12mm40Cr盘条和φ20~22mm40Cr圆钢.盘条和圆钢的钢质洁净,金相组织为铁素体+珠光体,性能满足《合金结构钢》(GB/T3077-2015)标准要求.盘条的拉伸性能:屈服强度ReL=914~1013MPa,抗拉强度Rm=1033~1090MPa,延伸率A=13.4%~18.8%,面缩率Z=55.6%~61.9%.圆钢的拉伸性能:屈服强度ReL=880~1000MPa,抗拉强度Rm=985~1070MPa,延伸率A=13.2%~16.7%,面缩率Z=52.8%~58.9%.