中国变形高温合金研制进展
Journal of Aeronautical Materials(2016)
Abstract
概述了近10年来我国变形高温合金的研制情况.介绍了航空发动机用涡轮盘材料718Plus,GH4720Li,GH4065合金的特点,燃烧室用GH3230合金以及燃气轮机用GH4706合金的研制进展.并对变形高温合金热加工新技术进行了总结,包括针对易偏析材料开发的ERS-CDS新工艺,改善变形高温合金棒材组织的反复镦拔工艺,提升高性能难变形高温合金热塑性的缓冷处理和热机械循环处理技术.最后,展望了我国变形高温合金产业的未来.
MoreTranslated text
Key words
wrought superalloy,slow cooling treatment,multi-cycle thermomechanical,double-phase superplastic