通过热压缩试验研究了5356铝合金在变形温度350~500℃和应变速率0.01~10 s-1的热成形性能,建立了5356铝合金本构方程和热加工图.结果 表明:5356铝合金高温变形过程主要受位错的热激活能控制;热变形最佳工艺参数是变形温度460~500℃,应变速率0.01~0.05 s-1;不稳定变形工艺参数是变形温度350~380℃和应变速率0.02~0.37 s-1以及变形温度420~500℃和应变速率0.14~10s-1.