K424高温合金显微组织和力学性能分析
Foundry Technology(2020)
Abstract
通过金相显微镜、扫描电镜研究了K424合金显微组织.研究表明:K424合金中主要为MC型碳化物和(γ+γ')共晶组织,MC型碳化物分为汉字骨架状和颗粒、长条状;汉字骨架状的MC型碳化物不利于提高合金伸长率和断面收缩率.