橡胶防老剂4020合成工艺的优化

Applied Chemical Industry(2014)

Cited 0|Views5
No score
Abstract
以Pt/MC作催化剂,对4020合成工艺条件进行了考察。结果表明,催化剂用量2%,酮胺摩尔比为3.0:1,反应温度100℃,压力3.0 MPa,搅拌转速400 r/min的条件下,可在短时间内得到较优产量和质量的4020。