疏浚底泥免烧裹壳骨料混凝土路面砖的性能研究

Pengqian YANG,Xinru AN,Yuzhou PENG, Yu WANG,Yan WU

New Building Materials(2018)

Cited 0|Views2
No score
Abstract
以疏浚底泥免烧裹壳骨料(WSLAs)和碎石骨料(CSAs)为粗骨料制备免烧裹壳骨料路面砖(WSLAB)和碎石骨料路面砖(CSB),对WSLAB和CSB的界面过渡区(ITZ)的微观形貌进行分析,分别铺设50块WSLAB和CSB至人行道上进行实际踩踏试验,并对路面砖踩踏200 d前后的耐候性进行对比.结果表明:WSLAs的筒压强度仅为CSAs的1/3,但WSLAB和CSB的抗压强度相近且均达到Cc30级实心砖的标准要求,吸水率、抗冻性符合GB/T 21144—2007,耐磨度和防滑性符合GB 28635—2012.与CSAs相比,WSLAs的"吸放水"特性使水泥石与WSLAs的结合力更强,其ITZ水化反应更完全.通过200 d的观测,WSLAB和CSB整体结构完整,均满足实际使用要求.