Lithium–Oxygen Power Source: the Influence of Positive Electrode Thickness on the Overall Discharge Characteristics

RUSSIAN JOURNAL OF ELECTROCHEMISTRY(2020)

引用 3|浏览0
暂无评分
摘要
Characteristic feature of the discharge process of lithium–oxygen battery cathode with non-aqueous electrolyte is the blockade of pores in the positive electrode by lithium peroxide (Li 2 O 2 ), an insoluble in the electrolyte and non-conductive substance. Lithium peroxide blocks cathode pores and thus hinders the oxygen entering therein. This complicates, in its turn, further behavior of the reaction. The goal of this work is to understand the following problems: (1) why is the acceptable thickness of the positive-electrode active layer extremely low, and (2) what is the reason of the lowering of specific capacity with the increasing of the active layer thickness. The main properties of the lithium—oxygen battery discharge—the current density, discharge time, specific capacity and the constant of oxygen consumption k *—were calculated using a digital simulation method. It was shown that the necessity of usage of low discharge current density is caused by the small thickness of the cathode region adjacent to the boundary with gaseous phase, in which the formation of Li 2 O 2 occurs. An increase in the cathode thickness induces a decrease in the current density, which, in its turn, leads to increase in parameter k and decrease in the discharge capacity.
更多
查看译文
关键词
cathode of lithium-oxygen battery,discharge process,theory of monoporous cathode,constant of oxygen consumptionk,current density
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要